Views: 0 Author: Site Editor Publish Time: 2025-09-26 Origin: Site
PC40 and PC95 are naming conventions for magnetic core materials by TDK. Their differences are mainly reflected in the following aspects:
PC40和PC95是TDK公司对磁芯材料的命名,它们的区别主要体现在以下几个方面 :
Permeability: The initial permeability of PC40 is generally around 2200–2300, while that of PC95 is 3300. With a higher permeability, PC95 can provide a stronger magnetic field strength under the same number of coil turns and dimensions.
- 磁导率:PC40的初始磁导率一般在2200-2300左右,而PC95的初始磁导率为3300,PC95磁导率更高,意味着在相同的线圈匝数和尺寸下,PC95磁芯能够提供更强的磁场强度。
Core Loss: Under conditions of 100°C, 100 kHz, and 200 mT, the core loss of PC40 is 420 kW/m³, whereas that of PC95 is 290 kW/m³. PC95 has lower core loss, which helps reduce heat generation and improve energy conversion efficiency.
- 磁芯损耗:在100℃、100kHz、200mT的条件下,PC40的磁芯损耗为420kW/m³,PC95的磁芯损耗为290kW/m³,PC95的磁芯损耗更低,能有效减少发热,提高能源转换效率。
Saturation Magnetic Flux Density: At 25°C, the saturation magnetic flux density of PC40 is 510 mT, and that of PC95 is 530 mT; at 100°C, PC40’s is 380 mT, and PC95’s is 410 mT. PC95 has a relatively higher saturation magnetic flux density and experiences a smaller change with temperature.
- 饱和磁通密度:在25℃时,PC40的饱和磁通密度为510mT,PC95为530mT;在100℃时,PC40的饱和磁通密度为380mT,PC95为410mT。PC95的饱和磁通密度相对较高,且随温度变化的幅度较小。
Curie Temperature: The Curie temperature of PC40 is greater than 200°C, while that of PC95 is greater than 215°C. With a higher Curie temperature, PC95 offers better thermal stability.
- 居里温度:PC40的居里温度大于200℃,PC95的居里温度大于215℃,PC95的居里温度更高,其热稳定性更好。
Price: Since PC95 has superior performance compared to PC40, its price is also relatively higher.